Polymer Property : Tensile Strength = 78.5 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 78.5 MPa
11400 psi
ASTM D638
Samyang Trirex® 3025GN10 Polycarbonate, Reinforced Flame Retardancy
PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3025GN10 is a reinforced flame retardant grade.Applications: LCD Panel Frame (dimensio..
Tensile Strength 78.5 MPa
11400 psi
ASTM D638
Gromax CCP PBT 6730-104F Glass/Mineral Filled
Product Description: PBT glass/mineral reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excellent w..