Polymer Property : Tensile Strength = 7880 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 54.3 MPa
7880 psi
ASTM D638
Saint-Gobain Meldin® 3110 Thermoplastic Bearing Material
3110 has a very low coefficient of friction and is particularly well suited for use with soft mating surface materials such as aluminum and soft stainless steel. Meldin® 3100 materials have exce..