Polymer Property : Tensile Strength = 8.260 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 8.260 MPa
1198 psi
Product Property; Arlon SQA-TMS-048
Arlon 910-10Rxx-P1 0.010" Cured, Self-Fusing Silicone Rubber
1.0 inch wide, 0.010" thick, red, rectangular cross-section, silicone self-fusing tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part number.De..
Tensile Strength 8.260 MPa
1198 psi
Silicone Property; ASTM D412
Arlon T3020-R004 0.020" (0.508 mm) Thick, 1" wide, Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate
Design/Construction: Side 1: Cured Fusible Silicone RubberSubstrate: 25% Sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester FilmArlon MOX-Tape® Fiberglass Reinforced T..
Tensile Strength 8.260 MPa
1198 psi
Silicone Property; ASTM D412
Arlon T4015-R004 0.015" (0.381 mm) Thick, 1" wide, Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate
Design/Construction: Side 1: Cured Fusible Silicone RubberSubstrate: 15% Sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester FilmArlon MOX-Tape® Fiberglass Reinforced T..
Tensile Strength 8.260 MPa
1198 psi
Silicone Property; ASTM D412
Arlon T3015-R004 0.015" (0.381 mm) Thick, 1" wide, Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate
Design/Construction: Side 1: Cured Fusible Silicone RubberSubstrate: 25% Sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester FilmArlon MOX-Tape® Fiberglass Reinforced T..