Polymer Property : Tensile Strength = 82.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 82.0 MPa
11900 psi
ASTM D638
Premix Premi-Glas® 2143-24 CR-SX Fiberglass Reinforced Thick Molding Compound
Premi-Glas® 2143-24 CR-SX is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves..
Tensile Strength 82.0 MPa
11900 psi
ASTM D638
Premix Premi-Glas® 2143-24 CR-SX-HT Fiberglass Reinforced Thick Molding Compound
Premi-Glas® 2143-24 CR-SX is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves..
Tensile Strength 82.0 MPa
11900 psi
at Yield; ISO 527-1/-2
Quadrant EPP Nylatron® GSM PA 6 + MoS2, cast (ISO Data)
Nylatron GSM contains finely divided particles of molybdenum disulphide to enhance its bearing and wear behaviour without impairing the impact and fatigue resistance inherent to unmodified cast nylo..
Tensile Strength 82.0 MPa
11900 psi
50 mm/min; ISO 527-1
Sax Polymers SAXAMID 126H Nylon 6, Injection Molding Grade
SAXAMID 126H is a general purpose polyamide 6 injection-molding-grade. Benefits are short cycle times and good release properties. Additionally it has a higher content of heat stabilizer which is p..
Tensile Strength 82.0 MPa
11900 psi
50 mm/min; ISO 527-1
Sax Polymers SAXAMID 126 Nylon 6, Injection Molding Grade
SAXAMID 126 is a general purpose polyamide 6 injection-molding-grade. Benefits are short cycle times and good release properties.Information provided by SAX Polymers
Tensile Strength 82.0 MPa
11900 psi
ISO 527
Azoty Tarnow™ Tarnamid® T-27 MF30 Polyamide 6 - Mineral Reinforced
30% Mineral filled, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High mechani..