Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 57.4 MPa @Temperature 23.0 °C |
8330 psi @Temperature 73.4 °F |
EN ISO 527 |
Ensinger TECASINT 3012 Polyimide, Ochre Brown (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |