Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 5.93 MPa | 860 psi | ASTM D412 |
Teknor Apex Telcar® OBC 4965F Thermoplastic Elastomer Notes: Telcar OBC has superior mechanical strength and higher elongation which will provide a tougher more durable finished product. Telcar OBC can be used in less demanding sealing applications. T.. |
|||
Tensile Strength | 5.93 MPa | 860 psi | Silicone Property; ASTM D412 |
Arlon 28561R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1528 FiberglassSide 2: Uncured Silicone RubberInterleave 2: PolyethyleneAppearance: Red silicone gum o.. |