Polymer Property : Tensile Strength = 88.29 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 88.29 MPa
12810 psi
ASTM D638
E-Polymers TEKAFIN® PH50G2 20% Glass Fiber Reinforced High Strength Compounded-PP
Modified PP: TEKAFIN is modified PP resins formulated with various fillers and modifiers. It has product lines for impact modified, glass fiber reinforced, inorganic filler reinforced and hybrids.I..