Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 61.0 MPa | 8850 psi | ISO 527 |
Lucite International Diakon® Rapide CLG 356B Enhanced Molding Acrylic Polymer Specially designed to reduce injection molding cycle times and therefore provide production cost benefits.Information provided by Lucite International |
|||
Tensile Strength | 61.0 MPa | 8850 psi | Volume Resistivity 4 [log(ohm-cm)] |
TIMCAL ENSACO™ 250G Conductive Carbon Black ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can.. |
|||
Tensile Strength | 61.0 MPa | 8850 psi | Volume Resistivity 6.3 [log(ohm-cm)] |
TIMCAL ENSACO™ 250G Conductive Carbon Black ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can.. |
|||
Tensile Strength | 61.0 MPa @Strain 25.0 %, Temperature 23.0 °C |
8850 psi @Strain 25.0 %, Temperature 73.4 °F |
50 mm/min; ISO 527-2 |
BASF Elastollan R 1000 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |