Polymer Property : Tensile Strength = 8900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 61.4 MPa
8900 psi
ASTM D638
Techmer ES Luriblend® PA6/6 TS20 HS Nylon 66
Availability: North AmericaForms: PelletsAdditive: Heat Stabilized, PTFE Lubricant(18%) and Silicone Lubricant (2%)Features: Lubricated, Good Wear Resistance and Heat StabilizedInformation provide..
Tensile Strength 61.4 MPa
8900 psi
ASTM D638
Aaron Industries AAROPRENE® AEPC 5000-2 Engineered Polycarbonate Resin
Melt flow index may be specified.
Tensile Strength 61.4 MPa
8900 psi
cured
Atom Adhesives AA-DUCT 906 Epoxy Adhesive
AA-DUCT 906 represents the newest technology since the introduction of electrically conductive silver compounds. This unique formulation is based on a silver coated ceramic that results in lower mat..