Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 9.43 MPa | 1370 psi | ASTM D412 |
Elastocon TPE Technologies Elastocon® 8078B Thermoplastic Elastomer Elastocon® 8078B is a black thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8078B is well suited for consumer goods a.. |