Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 9.73 MPa | 1410 psi | After Heat Aging 158 hrs at 150°C; ASTM D412 |
Kraton® G7705 GI-B (SEBS) Compound Description: Kraton G7705 GI-B is an easy processing, general purpose 44 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Tensile Strength | 9.73 MPa | 1410 psi | After Heat Aging 158 hrs at 150°C; ASTM D412 |
Kraton® G7705 GI-N (SEBS) Compound Description: Kraton G7705 GI-N is an easy processing, general purpose 44 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |