Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 9.79 MPa | 1420 psi | 20 in/min; ASTM D638 |
Teknor Apex Sinvicomp SHM 4500 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Ethylene Oxide Sterilizable Uses: Medical/Healthcare Applications Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Tensile Strength | 9.79 MPa | 1420 psi | 20 in/min; ASTM D638 |
Teknor Apex Sinvicomp SME 8510 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Ethylene Oxide Sterilizable Uses: Medical/Healthcare Applications Forms: Granules Processing Method: ExtrusionInformation Provided by Teknor Apex |