Polymer Property : Tensile Strength = 91.7 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 77.9 - 91.7 MPa
11300 - 13300 psi
Bulk Molding Compounds BMC T45HT Automotive Grade Molding compound
BMC T45HT was designed for the very demanding applications of automotive under hood engine covers. It meets the GMP UP .007 specification for automotive under hood. BMC T45HT is a vinyl ester base..