Mechanical Properties Metric English Comments
Tensile Strength 63.4 MPa
9200 psi
ASTM D638
Saint-Gobain Meldin® 7003 CM Compression Molded MoS2 Filled Polyimide
Melidin® 7003 CM is a compression molded polyimide that includes 15% molybdenum disulfide self-lubricating filler for wear applications that operate in a vacuum or in very dry conditions.Specific..