Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 64.746 MPa | 9390.6 psi | ASTM D638 |
E-Polymers TEKAMID® JN110 PPE+PA66 Filler Reinforced PA/PPE Alloy Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.JN-series: PA66/PPE, PA6/P.. |