Polymer Property : Tensile Strength = 960 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 6.62 MPa
960 psi
Silicone Property; ASTM D412
Arlon HSLW401R##-P0 0.040" (1.02 mm) Self-Fusing Silicone Tape (Triangular, Unsupported)
Description: High Strength, 1 inch wide, 40 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicate..