Tensile Strength 67.6 MPa
9800 psi
ASTM D-638
Plaskolite Optix® CP - 81 General Purpose Acrylic Resin
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli..
Tensile Strength 67.6 MPa
9800 psi
ASTM D-638
Plaskolite Optix® CP - 82 General Purpose Acrylic Resin
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli..
Tensile Strength 67.6 MPa
9800 psi
ASTM D-638
Plaskolite Optix® CP - 82 UVA General Purpose Acrylic Resin
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli..
Tensile Strength 67.6 MPa
9800 psi
ASTM D-638
Plaskolite West Optix® CP - 81 General Purpose Acrylic Resin
Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av..
Tensile Strength 67.6 MPa
9800 psi
ASTM D-638
Plaskolite West Optix® CP - 82 UVA General Purpose Acrylic Resin
Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av..
Tensile Strength 67.6 MPa
9800 psi
Cross; ASTM D882
Arlon CuClad 233 PTFE/Woven Fiberglass Laminate Microwave Printed Circuit Board Substrate
CuClad 233 uses a medium fiberglass/PTFE ratio to balance lower dielectric constant and improved dissipation factor without sacrificing mechanical properties.Cross Plied Woven Fiberglass, alternatin..
Tensile Strength 67.6 - 81.4 MPa
9800 - 11800 psi
Bulk Molding Compounds BMC HT12-1026 Unsaturated Polyester Bulk Molding Compound
BMC HT12-1026 is a highly engineered Unsaturated Polyester Bulk Molding Compound developed for automotive under-hood applications. This compound is specified by Ford motor company for solenoid caps..
Tensile Strength 67.6 - 81.4 MPa
9800 - 11800 psi
Bulk Molding Compounds BMC HT12-1023L Unsaturated Polyester Bulk Molding Compound
BMC HT12-1023L is a highly engineered Unsaturated Polyester Bulk Molding Compound developed for automotive under-hood applications. This compound is specified by Ford motor company for solenoid cap..
Tensile Strength 67.6 MPa
9800 psi
ASTM D-638
Plaskolite West Optix® CP - 82 General Purpose Acrylic Resin