Mechanical Properties Metric English Comments
Tensile Strength 6.83 MPa
990 psi
ASTM D412
Teknor Apex Telcar® OBC 4965A Thermoplastic Elastomer
Notes: Telcar OBC has superior mechanical strength and higher elongation which will provide a tougher more durable finished product. Telcar OBC can be used in less demanding sealing applications. T..