Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 0.193 MPa | 28.0 psi | 25% Deformation; 2.0 pcf density |
NOVA Chemicals Arcel 730 70% PS/30% PE Interpolymer ARCEL is a high-performance, moldable foam resin consisting of 70% polystyrene (PS) and 30% polyethylene (PE). ARCEL provides toughness, flexibility and durability in a lightweight foam.The strength.. |
|||
Compressive Strength | 0.193 MPa | 28.0 psi | 5% Deformation; Fired |
Unifrax Fiberfrax® Duraboard® 500ES Ceramic Fiber Board Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard .. |