Mechanical Properties Metric English Comments
Compressive Strength 0.207 MPa
30.0 psi
25% Compression, Deflection
3M Cushion-Mount™ 1015 Plus Plate Mounting Tape
3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr..
Compressive Strength 0.207 MPa
30.0 psi
25% Compression, Deflection
3M Cushion-Mount™ 1020R Plus Plate Mounting Tape
3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr..
Compressive Strength 0.207 MPa
30.0 psi
25% Compression, Deflection
3M Cushion-Mount™ E1015 Plus Plate Mounting Tapes with Easy Mount Adhesive
3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel..
Compressive Strength 0.207 MPa
30.0 psi
25% Compression, Deflection
3M Cushion-Mount™ E1020 Plus Plate Mounting Tapes with Easy Mount Adhesive
3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel..
Compressive Strength 0.207 MPa
30.0 psi
10% Compression, Deflection
3M Cushion-Mount™ E1715 Plus Plate Mounting Tapes with Easy Mount Adhesive
3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel..
Compressive Strength 0.207 MPa
30.0 psi
25% Compression, Deflection
3M Cushion-Mount™ 1015M Plus Plate Mounting Tape
3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr..
Compressive Strength 0.207 MPa
30.0 psi
25% Compression, Deflection
3M Cushion-Mount™ 1020 Plus Plate Mounting Tape
3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr..
Compressive Strength 0.207 MPa
30.0 psi
25% Compression, Deflection
3M Cushion-Mount™ 1020M Plus Plate Mounting Tape
3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr..
Compressive Strength 0.207 MPa
30.0 psi
10% Compression, Deflection
3M Cushion-Mount™ 1720M Plus Plate Mounting Tape
3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr..
Compressive Strength 0.207 MPa
30.0 psi
10% Compression, Deflection
3M Cushion-Mount™ E1720 Plus Plate Mounting Tapes with Easy Mount Adhesive
3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel..