Polymer Property : Compressive Strength = 0.221 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 0.221 MPa
32.0 psi
50% deformation
Unifrax Fiberfrax® Roll Board Ceramic Fiber Paper
The lower density, binder chemistry, and bulk ceramic fiber grade used to manufacture Fiberfrax Rollboard paper result in a product with lower cost, higher flexibility, and reduced smoke and odor du..
Compressive Strength 0.221 MPa
32.0 psi
10% Deformation; Fired
Unifrax Fiberfrax® Duraboard® 350ES Ceramic Fiber Board
Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard ..
Compressive Strength 0.221 MPa
32.0 psi
15% Deformation; Fired
Unifrax Fiberfrax® Duraboard® HD Ceramic Fiber Board
Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard ..