Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 0.524 MPa
76.0 psi
15% Deformation; Green
Unifrax Fiberfrax® Duraboard® 500ES Ceramic Fiber Board
Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard ..
Compressive Strength 0.524 MPa
76.0 psi
15% Deformation; Green
Unifrax Fiberfrax® Duraboard® 350ES Ceramic Fiber Board
Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard ..