Mechanical Properties Metric English Comments
Compressive Strength 10.0 MPa
1450 psi
(C 165)
Pyrotek Pyrite B-3 Refractory Board
Pyrotek B-3 is a highly versatile calcium silicate board for use in a variety of machined shapes and general purpose applications. Among its uses, Pyrotek B-3 is established as the industry standar..
Compressive Strength 10.0 MPa
1450 psi
1% Yield Point; DIN 53454
Fluorseals PTFE Unfilled
Information provided by TEKU GmbH Fluorkunststoffe, a distributor of Fluorseals materials.
Compressive Strength 10.0 MPa
1450 psi
EN 1094-5: 1995
Skamol Group Moler ROTOL Insulating Block
SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str..
Compressive Strength 10.0 MPa

@Time 36.0 sec
1450 psi

@Time 0.0100 hour
Wolf Kunststoff ZEDEX® ZX-550PV A7A Polymer Alloy
Main Characteristics: Modified friction wear; Tough; Soft; Reduced wear at temperatures at 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsInfor..
Compressive Strength >= 10.0 MPa

@Temperature 23.0 °C,
Time 86400 sec
>= 1450 psi

@Temperature 73.4 °F,
Time 24.0 hour
@ 1% deformation, 140 Kg/cm<sup>2</sup>; ASTM D621
Adamas Adalon® 103 PTFE, 10% Carbon Filled
Information provided by Adamas, HPM
Compressive Strength >= 10.0 MPa

@Temperature 23.0 °C,
Time 86400 sec
>= 1450 psi

@Temperature 73.4 °F,
Time 24.0 hour
@ 1% deformation, 140 Kg/cm<sup>2</sup>; ASTM D621
Adamas Adalon® 118 PTFE, 23/2% Carbon/Graphite Filled
Information provided by Adamas, HPM
Compressive Strength 10.0 MPa
1450 psi
measured on material fired at 370°C
Pyrotek ISOCAST Insulating Refractory Castable
Pyrotek's Isocast is a refractory castable based on phosphate bonded calcium silicate material. Isocast exhibits excellent thermal insulation characteristics and very good behavior with respec..
Compressive Strength 10.0 MPa
1450 psi
Pyrotek Pyrocast SC-2600 Refractory Cast Parts
Resistant to metal and flame abrasion, Pyrocast SC-2600 is the recommended castable refractory for applications such as filter box frames, burner tubes and troughs. The high purity silicon carbide ..