Mechanical Properties Metric English Comments
Compressive Strength 0.689 MPa
100 psi
SPHERE ONE EXTENDOSPHERESâ„¢ XOL-150 Hollow Spheres
EXTENDOSPHERESâ„¢ XOL-150 are white aluminosilicate multicellular hollow spheres. The density of this product is 0.30 g/cc. In plastic and coating applications, EXTENDOSPHERESâ„¢ XOL-150 hollo..