Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Strength = 118 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 118 MPa
17100 psi
Pyrotek NAD-11 Structural Insulation Board
NAD-11 is an asbestos-free cement board with excellent electrical properties. It has a high density cement board reinforced with inorganic fibers.ApplicationsCathode support pads Platen insulation ..
Compressive Strength 118 MPa
17100 psi
Pyrotek NAD-500 Electrical Insulation Product
Cement reinforcement, Inorganic fiber resinApplicationsSuperstructure support pads Bus bar insulators Pot cradle insulators Exhaust duct insulators Machined parts Wedges & shunts Point feeder gasket..
Compressive Strength 118 MPa
17100 psi
Poco Graphite TRA Semiconductor Grade Graphite
Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their ..
Compressive Strength 118 MPa
17100 psi
ASTM D695
Solvay Specialty Polymers AvaSpire® AV-848 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire® AV-848 is a high-temperature, polyaryletherketone (PAEK) that offers several key performance advantages over comparable grades of PEEK above 150°C, including better dimensional stability..
Compressive Strength 118 MPa
17100 psi
ASTM D695
Solvay Specialty Polymers KetaSpire® KT-820 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire PEEK is produced to the highest industry standards and is characteriz..
Compressive Strength 118 MPa
17100 psi
ASTM D695
Solvay Specialty Polymers AvaSpire® AV-848 Polyaryletherketone (PAEK)
AvaSpire® AV-848 is a high-temperature, polyaryletherketone (PAEK) that offers several key performance advantages over comparable grades of PEEK above 150°C, including better dimensional stabi..
Compressive Strength 118 MPa
17100 psi
ASTM D695
Solvay Specialty Polymers KetaSpire® KT-820 Polyetheretherketone (PEEK)
KetaSpire® KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire® PEEK is produced to the highest industry standards and is cha..
Compressive Strength 118 MPa
17100 psi
ASTM D695
Solvay Specialty Polymers KetaSpire® KT-XXXX Polyetheretherketone (PEEK)
KetaSpire® KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire® PEEK is produced to the highest industry standards and is cha..
Compressive Strength 118 MPa
17100 psi
Cold Crushing
Sharadaa Ceramics PCF (AZS) Precast Prefired Brick
Features: Manufactured under controlled conditions under refractory engineers supervision; Measured Quantity/Temperature of water, mixing by Intensive counter current mixers, Forming by Vibro Castin..
Compressive Strength 118 MPa
17100 psi
ASTM D695
Ensinger Tecapeek® Polyetheretherketone (PEEK)
Tecapeek™, made from Victrex PEEK polymer, is an excellent material for a wide spectrum of applications where thermal, chemical, and combustion properties are critical to performance.Excellent flex..
Compressive Strength 118 MPa

@Temperature 22.8 °C
17100 psi

@Temperature 73.0 °F
ASTM D695
Ensinger Tecapeek® Polyetheretherketone (PEEK)
TECAPEEK™ high performance polymer, made from Victrex PEEK polymer, has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's excepti..
Compressive Strength 118 MPa
17100 psi
Cold Crushing Strength
Chosun Refractories AC-1 Acid-Proof and Heat-Resistant Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 118 MPa
17100 psi
Cold Crushing Strength
Chosun Refractories SB85S Bricks, Oxide Bonded SiC
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 118 MPa
17100 psi
Cold Crushing Strength
Chosun Refractories SBSN20 Nozzle
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 118 MPa
17100 psi
Abatron AboCast 22-30/AboCure 50-12 Epoxy
AboCast 22-30 is a black filled resin with high viscosity and a weight of 12.4 lbs/gallon. AboCure 50-12 is clear, fast converter with low viscosity and a weight of 8.2 lbs/gallon. AboCast 22-30/Abo..
Compressive Strength 118 MPa
17100 psi
ASTM D695
ScanTube PEEK Tubing
Information provided by ScanTube, Inc.
Copyright © lookpolymers.com All Rights Reserved