Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Strength = 12300 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 85.0 MPa
12300 psi
Cold Crushing Strength
Gouda Vuurvast AK 90 Dense Refractory Brick
Description: This brick can be used in very severe conditions, i.e. in reducing atmosphere at a high temperatures, e.g. in carbon-black furnaces.Remarks: This data represents average values, obtaine..
Compressive Strength 85.0 MPa
12300 psi
ASTM D362
Unitika M1030B PA6, Dry
Nano composite nylonInformation provided by Unitika Ltd.
Compressive Strength 84.8 MPa
12300 psi
Engineered Syntactic Systems AZ-38 Deep Water Syntactic Foam
Syntactic foams are a combination of hollow spheres, a resin matrix, and other additives. When combined and processed properly, the constituents form a lightweight homogeneous material having high c..
Compressive Strength 85.0 MPa
12300 psi
Absolute Drying; ASTM-D695
Toyobo GLAMIDE® T-803 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Compressive Strength 84.8 MPa
12300 psi
ASTM D695
Ensinger Hydel® PC-7 Polycarbonate (PC)
A polycarbonate based material with a proprietary carbon filler component. The highly dispersed filler imparts outstanding electrical consistency to minimize any hot spots. The material has good r..
Compressive Strength 85.0 - 100 MPa
12300 - 14500 psi
GB/T 1040
Beijing Evergrow Resources Oilon
Information provided by Beijing Evergrow Resources.
Compressive Strength 84.8 - 112 MPa
12300 - 16300 psi
Bulk Molding Compounds BMC T60 Grey Wear Resistant Molding Compound
BMC T60 Grey is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cost per cu..
Compressive Strength 85.0 - 100 MPa
12300 - 14500 psi
GB/T 1040
Beijing Evergrow Resources Enylon®
Information provided by Beijing Evergrow Resources.
Compressive Strength 85.0 - 100 MPa
12300 - 14500 psi
GB/T 1040
Beijing Evergrow Resources MC Nylon
Information provided by Beijing Evergrow Resources.
Compressive Strength 84.8 - 112 MPa
12300 - 16300 psi
Bulk Molding Compounds BMC T60-6006 Wear Resistant Molding Compound
BMC T60-6006 is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cost per cu..
Copyright © lookpolymers.com All Rights Reserved