Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 1250 MPa | 181000 psi | HRC 45 R<sub>c</sub>0.2 |
Assab Steels DF-3 Cold Work Steel DF-3 general purpose oil-hardening tool steel is a versatile manganese-chromium-tungsten steel suitable for a wide variety of cold-work applications. Its main characteristics include:Good machinabil.. |