Compressive Strength 0.981 - 1.47 MPa
142 - 213 psi
Cold Crushing
Sharadaa Ceramics CFI Insulation Brick
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..
Compressive Strength <= 0.981 MPa
<= 142 psi
Cold Crushing Strength
Chosun Refractories A-7 Insulating Firebrick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength <= 0.981 MPa
<= 142 psi
Cold Crushing Strength
Chosun Refractories LW-24 Special Insulating Firebrick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength <= 0.981 MPa
<= 142 psi
Cold Crushing Strength
Chosun Refractories LW-28 Special Insulating Firebrick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength <= 0.981 MPa
<= 142 psi
Cold Crushing Strength
Chosun Refractories A-6 Insulating Firebrick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 0.981 MPa
142 psi
Cold Crushing Strength
Chosun Refractories CFA-1 Ceramic Foam
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 0.981 MPa
142 psi
Cold Crush Strength
BNZ Materials PA 23 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Compressive Strength 0.981 MPa
142 psi
Cold Crushing
Sharadaa Ceramics 0.4 Insulation Brick
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..