Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 9.81 - 10.3 MPa | 1420 - 1490 psi | 1% Deformation; ASTM D695 |
Polikim EFALON® B-40 PTFE, 40% Bronze Filled Bronze-filled Efalon® (PTFE) has better heat insulation, less thermal expansion, higher wear resistance properties and less deformation under load compared to virgin Efalon®. Applications: bearing.. |
|||
Compressive Strength | <= 9.81 MPa | <= 1420 psi | Cold Crushing Strength |
Chosun Refractories C-3 Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 9.81 - 19.6 MPa @Temperature 1350 °C, Time 10800 sec |
1420 - 2840 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories TG-55 Monolithic Refractories for Ladle and Tundish Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 9.81 MPa @Temperature 1500 °C, Time 10800 sec |
1420 psi @Temperature 2730 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories TG-68 Monolithic Refractories for Ladle and Tundish Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |