Polymer Property : Compressive Strength = 14400 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 99.3 MPa
14400 psi
ASTM D695
Solvay Specialty Polymers Torlon® 4630 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4630 is an injection-moldable, wear-resistant grade of polyamide-imide (PAI), that has been formulated to give outstanding wear resistance in non-lubricated applications. Torlon PAI has the h..
Compressive Strength 99.3 MPa
14400 psi
ASTM D695
Solvay Specialty Polymers Torlon® 4630 Polyamide-imide (PAI)
Torlon® 4630 is an injection-moldable, wear-resistant grade of polyamide-imide (PAI), that has been formulated to give outstanding wear resistance in non-lubricated applications. Torlon® PAI h..
Compressive Strength 99.0 MPa

@Time 360000 sec
14400 psi

@Time 100 hour
Wolf Kunststoff ZEDEX® ZX-410 A4A Polymer Alloy
ZX-410 is a bearing material with excellent properties and a very affordable price.Main Characteristics: Hard, Stiff, Tough; High dimensional stability; High chemical resistance; High water resistan..
Compressive Strength 99.3 MPa
14400 psi
BCC Products BC 7062H Epoxy Casting
BC 7062 are aluminum filled, low viscosity epoxy mass casting resins. These room temperature cure systems allow the user choice thicknesses of 1/8 inch to a maximum of 6 inches without foaming or yi..