Mechanical Properties Metric English Comments
Compressive Strength 151 MPa
21900 psi
1.3 mm/min; ASTM D695
Lavergne VYPET VNT 340 PET 40% Glass - Mineral Reinforced
Vypet VNT 340 is a 40% glass/mineral reinforced PET injection molding compound designed for electrical and structural applications, with High Dielectric StrengthFeatures: High temperature performanc..
Compressive Strength 151 MPa
21900 psi
ASTM D695
Plenco 00714 Melamine-Phenolic, Granular, Injection Molded
PLENCO 00714 is a melamine-phenolic copolymer molding compound, offering excellent arc resistance and comparative track index values. Type ASTM D 5948 CMG, and UL recognized under component file E4..
Compressive Strength 151 MPa
21900 psi
ASTM D695
Ensinger TECAPEI® made from Ultem® 1000 PEI
TECAPEI™ is an amorphous thermoplastic polyetherimide (PEI) made from Sabic Innovative Plastics' Ultem® 1000 and 2000 series resins. The unreinforced 1000 series materials are translucent amber in..