Compressive Strength 154 MPa
22300 psi
10% Def.; ASTM D695
Quadrant EPP Semitron® 420 ESd V (ASTM Product Data Sheet)
Compressive Strength 154 MPa
22300 psi
Master Bond EP112 Low Viscosity Heat Curing Cycloaliphatic Epoxy Adhesive
Master Bond Polymer System EP112 is a solventless, low viscosity two component cycloaliphatic epoxy resin system which is specifically designed for high performance outdoor and indoor electrical & e..