Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 1540 MPa @Temperature 23.9 °C |
223000 psi @Temperature 75.0 °F |
Dry; ASTM D695 |
Park Electrochemical Nelcote® E-718 Epoxy Prepreg, G30-700 Uni-Tape Reinforced Nelcote® E-718 is a modified epoxy resin system. E-718 is designed to provide excellent mechanical properties at low cure pressures.Key Features and Benefits:Good low pressure consolidationExcellen.. |
|||
Compressive Strength | 1540 MPa | 224000 psi | |
Universal Wire Works No. 6 Cobalt Alloy Welding Wire Universal No. 6 is a cobalt-chromium-tungsten alloy suited for applications requiring extreme impact resistance at elevated temperatures, exhaust valve contact surfaces, hot and cold trimmer dies an.. |