Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 107 MPa | 15500 psi | 10% Def.; ASTM D695 |
Quadrant EPP Techtron® HPV PPS (ASTM Product Data Sheet) |
|||
Compressive Strength | 107 MPa | 15500 psi | ASTM D695 |
PolyOne Edgetek® NY-20GF/10GB/000 Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Compressive Strength | 107 MPa | 15500 psi | ASTM D695 |
PolyOne Edgetek® NY-20GF/10GB/000 Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Compressive Strength | 107 MPa | 15500 psi | ASTM D695 |
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK)
(Unverified Data**) AV-722 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding wea.. |
|||
Compressive Strength | 107 MPa | 15500 psi | ASTM D695 |
Greene Tweed Arlon® 1330 PEEK Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie.. |
|||
Compressive Strength | 107 MPa | 15500 psi | ASTM D695 |
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK) AV-722 SL30 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding.. |
|||
Compressive Strength | 107 MPa | 15500 psi | 10% strain; ASTM D695 |
Saint-Gobain Meldin® 7211 Isostatically Molded Graphite and PTFE Filled Polyimide Finished parts and basic shapes made from 10% by weight PTFE and 15% by weight graphite filled polyimide material for applications requiring a very low coefficient of friction and self-lubricating p.. |
|||
Compressive Strength | 107 MPa @Time 360000 sec |
15500 psi @Time 100 hour |
|
Wolf Kunststoff ZEDEX® ZX-324 A3A PEEK Main Characteristics: Hard; Stiff; Tough; High fatigue strength; Good water resistance; Sufficient UV and weather resistance; Flame retardant; Good machinability; FDA compliant LABS; PTFE and Silico.. |
|||
Compressive Strength | 107 MPa | 15500 psi | |
3M Scotchkote™ EG 503 Epoxy Metal Repair Scotchkote Epoxy Metal Repair EG 503 is a specifically developed high performance metal compound that provides good mechanical strength combined with easy machining properties.Product Features:Combi.. |
|||
Compressive Strength | 107 MPa | 15500 psi | Crosswise; ASTM D635 |
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 1/8" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Compressive Strength | 107 MPa | 15500 psi | Crosswise; ASTM D635 |
Bedford Plastics Glass Reinforced Polyester Flat Sheet 1/8" Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |