Compressive Strength 1600 MPa
232000 psi
DIN 51067T1
CeramTec ZN 40 Zirconia, ZrO2-MgO
ZN 40 is a zirconium oxide ceramic with an excellent surface finish and a higher strength than aluminum oxide. Its good crack resistance and anti-friction properties, combined with steel-like therma..