Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 11.0 MPa | 1600 psi | EN 1094-5: 1995 |
Skamol Group VIP 12 Vermiculite Insulating Slab SKAMOL V-1100 & VIP-12 vermiculite slabs have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulation of all refractory constr.. |
|||
Compressive Strength | >= 11.0 MPa | >= 1600 psi | |
Engineered Syntactic Systems SF-22 Subsea Macrosphere Syntactic Void Filler In applications where density is critical, the four part SF-22 kit is used. This system utilizes fiber reinforced epoxy macrospheres in combination with the standard microsphere syntactic to provide.. |
|||
Compressive Strength | 11.0 MPa | 1600 psi | Elastic Limit |
Wolf Kunststoff ZEDEX® ZX-550PV A7A Polymer Alloy Main Characteristics: Modified friction wear; Tough; Soft; Reduced wear at temperatures at 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsInfor.. |
|||
Compressive Strength | 11.0 MPa @Temperature 25.0 °C |
1600 psi @Temperature 77.0 °F |
1% deformation; ASTM D695 |
Daikin NEOFLON EA-LR43 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Compressive Strength | 11.0 MPa @Temperature 25.0 °C |
1600 psi @Temperature 77.0 °F |
1% deformation; ASTM D695 |
Daikin NEOFLON EP-521 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Compressive Strength | 11.0 MPa @Temperature 25.0 °C |
1600 psi @Temperature 77.0 °F |
1% deformation; ASTM D695 |
Daikin NEOFLON EP-610 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Compressive Strength | 11.0 MPa @Temperature 25.0 °C |
1600 psi @Temperature 77.0 °F |
1% deformation; ASTM D695 |
Daikin NEOFLON EP-610AS ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Compressive Strength | 11.0 MPa @Temperature 25.0 °C |
1600 psi @Temperature 77.0 °F |
1% deformation; ASTM D695 |
Daikin NEOFLON RP-4020 EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
Compressive Strength | 11.0 MPa @Temperature 25.0 °C |
1600 psi @Temperature 77.0 °F |
1% deformation; ASTM D695 |
Daikin NEOFLON RP-4040 EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
Compressive Strength | 11.0 MPa @Temperature 25.0 °C |
1600 psi @Temperature 77.0 °F |
1% deformation; ASTM D695 |
Daikin NEOFLON RP-5000 EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
Compressive Strength | 11.0 MPa @Temperature 25.0 °C |
1600 psi @Temperature 77.0 °F |
1% deformation; ASTM D695 |
Daikin NEOFLON RP-5000AS EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
Compressive Strength | 11.0 MPa @Temperature 25.0 °C |
1600 psi @Temperature 77.0 °F |
1% deformation; ASTM D695 |
Daikin NEOFLON EP-620 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Compressive Strength | 11.0 MPa @Temperature 25.0 °C |
1600 psi @Temperature 77.0 °F |
1% deformation; ASTM D695 |
Daikin NEOFLON EP-541 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Compressive Strength | 11.0 MPa | 1600 psi | @ 0.2% Offset; ASTM D695 |
Technetics Group Texolon™ 8534 PTFE
(Unverified Data**) PTFE CharacteristicsChemical ResistanceThermal StabilityCryogenic PropertiesLow Coefficient of FrictionLow Surface EnergyLow Dielectric ConstantHigh Volume and Surface ResistivityFlame ResistanceApp.. |
|||
Compressive Strength | 11.0 MPa | 1600 psi | @ 1.0% Strain; ASTM D695 |
Technetics Group Texolon™ 8534 PTFE
(Unverified Data**) PTFE CharacteristicsChemical ResistanceThermal StabilityCryogenic PropertiesLow Coefficient of FrictionLow Surface EnergyLow Dielectric ConstantHigh Volume and Surface ResistivityFlame ResistanceApp.. |