Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Strength = 16100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 111 MPa

@Temperature 204 °C
16100 psi

@Temperature 400 °F
ASTM D695
Haysite H320 Polyester Composite
A thermoset polyester composite that offers superior energy efficiency, temperature control, and durability for high temperature mold and platen thermal applications. A proven, cost effective produ..
Compressive Strength 111 MPa
16100 psi
ASTM D695
Solvay Specialty Polymers AvaSpire® AV-621 Polyaryletherketone (PAEK)
AvaSpire® AV-621 is an unreinforced polyaryletherketone (PAEK) that offers improved ductility and impact strength relative to PEEK while retaining most of the key performance attributes of PEEK. ..
Compressive Strength 111 MPa
16100 psi
Elastic Limit
Wolf Kunststoff ZEDEX® ZX-410 A4A Polymer Alloy
ZX-410 is a bearing material with excellent properties and a very affordable price.Main Characteristics: Hard, Stiff, Tough; High dimensional stability; High chemical resistance; High water resistan..
Compressive Strength 111 MPa
16100 psi
ASTM D695
Solvay Specialty Polymers AvaSpire® AV-621 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-621 is an unreinforced polyaryletherketone (PAEK) that offers improved ductility and impact strength relative to PEEK while retaining most of the key performance attributes of PEEK. The ..
Copyright © lookpolymers.com All Rights Reserved