Polymer Property : Compressive Strength = 1750 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 1750 MPa
254000 psi
MarkeTech Zirconium Oxide Ceramic, Zirconia MgO Stabilized
Data provided by the supplier, MarkeTech International.Zirconium oxide is widely used and has superior high temperature properties. When combined with yttria the strength and fracture toughness is ..
Compressive Strength 1750 MPa
254000 psi
ASTM C773
CoorsTek Dura-Z™ MgO Partially Stabilized Zirconia
Thermal Shock Delta Tc = 350°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Compressive Strength 1750 MPa
254000 psi
ASTM C773
CoorsTek TTZ (Dura-Z™) MgO Partially Stabilized Zirconia
Thermal Shock Delta Tc = 350°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Compressive Strength 1750 MPa
254000 psi
Aremco AREMCOLOX™ 502-1900-MTTZ Dense MgO Partially Stabilized Zirconium Oxide
This grade offers a high level of fracture toughness for a zirconia material. Features include excellent fracture, corrosion, thermal shock, and wear resistance. Used for pump parts, valve component..