Mechanical Properties Metric English Comments
Compressive Strength 1.26 MPa
183 psi
32 hour silo aging time, 20 kg/m^3
Jackon JACKOCELL® R312 Expanded Polystyrene Packaging and Shape Molding
100% Polystyrene.Pre-expansionHigh density stability in pre-expansion, transportation and silo storage reduces opportunity losses through achieving typical lower average density during regular produ..