Polymer Property : Compressive Strength = 18800 psi
Polymer Property :
Compressive Strength =
18800 psi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Compressive Strength
130
MPa
18800
psi
ASTM D695
ITW Devcon Metal Repair Titanium Putty, Grey
Information provided by ITW Devcon