Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 0.131 MPa | 19.0 psi | 5% Deformation; Fired |
Unifrax Fiberfrax® Duraboard® 2600 Ceramic Fiber Board Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard .. |