Polymer Property : Compressive Strength = 19900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 137 MPa
19900 psi
Cold Crushing
Sharadaa Ceramics PCF60-1 Precast Prefired Brick
Features: Manufactured under controlled conditions under refractory engineers supervision; Measured Quantity/Temperature of water, mixing by Intensive counter current mixers, Forming by Vibro Castin..
Compressive Strength 137 MPa
19900 psi
ASTM D695
Sumitomo Bakelite North America FM 4005X4648 Fiberglass Reinforced Phenolic Novolac
FM 4005X4648 a fiberglass reinforced phenolic novolac molding compound formulated to increase thermal conductivity and electrical conductance. This material also exhibits low post mold shrinkage.In..