Mechanical Properties Metric English Comments
Compressive Strength 1.38 MPa
200 psi
SPHERE ONE EXTENDOSPHERESâ„¢ XOL-200 Hollow Spheres
EXTENDOSPHERESâ„¢ XOL-200 are white aluminosilicate multicellular hollow spheres. The density of this product averages 0.25 g/cc. In plastic and coating applications, EXTENDOSPHERESâ„¢ XOL-200..