Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 1.50 MPa | 218 psi | 1% strain over 1000 hours; ISO.899 DIN.53444 |
Omnia Plastica PTFE Polytetrafluoroethylene A Fluoropolymer used mainly for its excellent chemical resistance. It has poor mechanical features. The strain, even under low weight, makes it very suitable as a gasket material.Features:Chemical: .. |
|||
Compressive Strength | 1.50 MPa @Thickness 19.0 mm |
218 psi @Thickness 0.750 in |
perpendicular to plane; ASTM C365 |
3A Composites Core Materials AIREX® PXw.320 Fiber-Reinforced Structural Foam Panel AIREX® PXw is a closed-cell, fiber reinforced polymer foam panel with a special formulation and very high mechanical properties. The sophisticated manufacturing process evenly distributes continuou.. |
|||
Compressive Strength | 1.50 MPa | 218 psi | average; perpendicular to plane; ISO 844 |
3A Composites Core Materials AIREX® C71.75 Elevated Temperature Structural Foam AIREX® C71 is a closed cell, crosslinked polymer foam especially formulated to maintain its stability also at higher processing or service temperatures. It combines excellent stiffness and strength.. |