Polymer Property : Compressive Strength = 230 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 200 - 230 MPa
29000 - 33400 psi
ISO 604
Vyncolit 2923 W Novolac Phenolic
Mineral filled phenolic molding compound with excellent heat resistance and dimensional stability.Information provided by Vyncolit, a Sumitomo Bak Group
Compressive Strength 200 - 230 MPa
29000 - 33400 psi
ISO 604
Vyncolit 4451 XB Novolac Phenolic
Organic and mineral filled phenolic molding compound with excellent mechanical properties (highest notched impact strength).USES: Fuse holders, brush holders, circuit breakers, automotive ignition a..
Compressive Strength 200 - 230 MPa
29000 - 33400 psi
ISO 604
Vyncolit 2530 W Novolac Phenolic
Mineral and organic filled phenolic molding compound with excellent thermal properties.USES: Lamp sockets, special lamp holders, pan handles and knobs.Information provided by Vyncolit, a Sumitomo Ba..
Compressive Strength 200 - 230 MPa
29000 - 33400 psi
ISO 604
Vyncolit 2723 W Novolac Phenolic
Mineral and organic filled phenolic molding compound with excellent mechanical, thermal and dielectric properties. I2/FO classified under NF F 16-101 (Fire & Smoke classification).USES: Circuit bre..
Compressive Strength 200 - 230 MPa
29000 - 33400 psi
ISO 604
Vyncolit 2920 W Novolac Phenolic
Mineral and organic filled molding compound with good dimensional stability and heat resistance.USES: Carburettor and intake manifold thermal insulator.Information provided by Vyncolit, a Sumitomo B..