Mechanical Properties Metric English Comments
Compressive Strength 159 MPa
23000 psi
SGL Carbon Group EK 203 Graphite
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
Compressive Strength 159 MPa
23000 psi
SGL Carbon Group EK 2230 Carbon Graphite
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
Compressive Strength 159 - 172 MPa
23000 - 25000 psi
Bulk Molding Compounds BMC 1454 for Injection Molding Circuit Breakers
BMC 1454 is a special low-cost material developed specifically for injection molding circuit breakers. It has considerable flame, arc and track resistance. BMC 1454 is a medium strength material wit..
Compressive Strength 159 - 193 MPa
23000 - 28000 psi
Bulk Molding Compounds BMC 695 Vinyl Ester Molding Compound
BMC 695 vinyl ester molding compound is a mineral filled glass fiber-reinforced vinyl ester compound suitable for compression and injection molding It is characterized by good moldability, oil and s..
Compressive Strength 159 MPa
23000 psi
Ultimate; TM R050-38
Resinlab® EP1306 Acrylic / Epoxy Hybrid Adhesive
EP1306 is a two part acrylic / epoxy hybrid adhesive utilizing a 50% weight loading of aluminum powder into both components. It cures quickly at room temperature to a tough, rigid polymer. It has go..
Compressive Strength 158.6 MPa
23000 psi
Henkel Hysol EA 9394 Paste Adhesive System
Thixotropic adhesive with structural properties to 350°F / 177°C.Applications: Potting Structural Repair Composite Bonding Liquid Shim