Polymer Property : Compressive Strength = 2310 MPa
Polymer Property :
Compressive Strength =
2310 MPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Compressive Strength
2310
MPa
335000
psi
ASTM C773
CoorsTek Alumina-Zirconia Composite, AZ-25
Information provided by CoorsTek.