Compressive Strength | 238 MPa | 34500 psi | ASTM D695 |
Saint-Gobain Meldin® 5330 Thermoplastic Bearing Material General Notes on Meldin 3000/5000 Series Bearing Products:Injection Moldable, High-Performance Bearings. Can withstand environments of high temperature, corrosive, and water.Specific Notes on Meldin.. |