Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 2414 MPa
350100 psi
ASTM C-773-88 / DIN 51067T1
CeramTec 614/698 Alumina, 96%
614/698 (96%) is a high-strength alumina with good mechanical properties, as well as good wear and chemical resistance. It also features excellent electrical properties. 614 is white; 698 is pink.