Mechanical Properties Metric English Comments
Compressive Strength 2500 MPa
363000 psi
DIN 51067T1
CeramTec V 38 Alumina, 96.0% Al2O3-SiO2
Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures.
Compressive Strength 2500 MPa
363000 psi
DIN 51067T1
CeramTec V 679 Alumina, 99.7%
Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures.
Compressive Strength 2500 MPa
363000 psi
ASTM C773
CoorsTek AD-998 Alumina(nom. 99.8% Al2O3)
Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Compressive Strength 2500 MPa
363000 psi
ASTM-C773
CoorsTek CAP 4 98.5% Alumina Ceramic Armor Material
CoorsTek CeraShield™ ceramics provide: low weight, high hardness, controlled, uniform microstructure, dimensional stability over wide temperature range, compatibility for use in finished armor sys..
Compressive Strength 2500 MPa
363000 psi
ASTM-C773
CoorsTek FG-98 98% Alumina Ceramic Armor Material
CoorsTek CeraShield™ ceramics provide: low weight, high hardness, controlled, uniform microstructure, dimensional stability over wide temperature range, compatibility for use in finished armor sys..
Compressive Strength 2500 MPa
363000 psi
ASTM C773
CoorsTek FG-995 Alumina (nom. 98.5% Al2O3)
Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Compressive Strength 2500 MPa
363000 psi
ASTM C773
CoorsTek Reaction Bonded Silicon Carbide, SCRB (SC-2)
Thermal Shock Delta Tc = 400°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Compressive Strength 2500 MPa
363000 psi
ASTM C773
CoorsTek Yttria Partially Stabilized Zirconia, YZTP, Sintered
Thermal Shock Delta Tc = 350°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Compressive Strength 2500 MPa
363000 psi
ASTM C773
CoorsTek YZTP Yttria Partially Stabilized Zirconia, Hipped
Thermal Shock Delta Tc = 350°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Compressive Strength 2500 MPa
363000 psi
Rc0.2; at HRC=60
Bohler-Uddeholm UDDEHOLM Vancron 40 nitrided powder tool steel
Description: Uddeholm Vancron 40 is a nitrided powder tool steel, which means that a “surface coating” is already integrated into the finished tooling material. The result is a tool surface with v..
Compressive Strength 2500 MPa
363000 psi
Rcm. Hardness HRC 58.
Assab Steels CALMAX Plastic Mold Material
CALMAX is a chromium-molybdenum-vanadium alloyed steel characterized by:High toughnessGood wear resistanceGood through hardening propertiesGood dimensional stability in hardeningGood polishabilityGo..
Compressive Strength 2500 MPa
363000 psi
Aremco AREMCOLOX™ 502-1900-YTZP Dense Yttria Stabilized Zirconium Oxide
This grade offers a high flexural strength for a zirconia. The fine grain size lends itself to be used in cutting tools where a very sharp edge can be achieved and maintained due to its high wear re..